CNT témbok tunggal, bubuk SWCNT: D: 2nm L: 1-2um / 5-20um
CNT témbok ganda, bubuk DWCNT: D: 2-5nm L: 1-2um / 5-20um
Multi walled CNT, bubuk MWCNT:
D: 10-30nm / 30-60nm / 60-100nm
L: 1-2um / 5-20um
Ngaropea jasa: COOH Functionalized;OH Fungsi;Dispersi Cai;Disperserions minyak;Nanotube Karbon Dilapis Nikel
Harta | Unit | DWCNTs | Métode Pangukuran | |||||
OD | nm | 2-4 | 2-4 | 2-4 | HRTEM, Raman | |||
Kasucian | beurat% | > 60 | > 60 | > 60 | TGA & TEM | |||
Panjangna | mikron | ~50 | ~50 | ~50 | TEM | |||
SSA | m2/g | >340 | > 350 | > 350 | BET | |||
lebu | beurat% | <5 | <5 | <5 | TGA | |||
Ig/Id | -- | -- | -- | -- | Raman | |||
-OH eusi | beurat% | 2.92 | XPS & Titrasi | |||||
- Kandungan COOH | beurat% | 2.58 | XPS & Titrasi | |||||
OD = Diaméter Luar SSA = Wewengkon Permukaan Spésifik |
Harta | Unit | SWCNTs pondok-Panjang | Métode Pangukuran | ||
OD | nm | 1-2 | 1-2 | 1-2 | HRTEM, Raman |
Kasucian | beurat% | >90 | >90 | >90 | TGA & TEM |
Panjangna | mikron | 1-3 | 1-3 | 1-3 | TEM |
SSA | m2/g | >340 | >380 | >380 | BET |
lebu | beurat% | <5 | <5 | <5 | HRTEM, TGA |
Ig/Id | -- | > 9 | > 9 | > 9 | Raman |
-OH Fungsional | beurat% | 3.96 | XPS & Titrasi | ||
-COOH Fungsional | beurat% | 2.73 | XPS & Titrasi | ||
OD = Diaméter Luar ID = Diaméter Batin SSA = Wewengkon Permukaan Spésifik |